Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 175 - 325 V | 175 - 325 V | Average value: 207 V Grade Count:17 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Comparative Tracking Index | 175 - 325 V | 175 - 325 V | Average value: 236 V Grade Count:7 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |