Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 155 V @Thickness 3.17 mm |
155 V @Thickness 0.125 in |
ASTM D3638 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Comparative Tracking Index | 155 V | 155 V | IEC test |
Toyobo TS301 PPS, 30% Glass Fiber Reinforced Key Feature: Excellent impact resistance, high flowHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo.. |