Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 33 - 36 MGOe | 33 - 36 MGOe | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 33 - 36 MGOe | 33 - 36 MGOe | |
Alliance N-35H Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 33 - 36 MGOe | 33 - 36 MGOe | |
Alliance N-35M Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 33 - 36 MGOe | 33 - 36 MGOe | |
Alliance N-35SH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 33 - 36 MGOe | 33 - 36 MGOe | |
Alliance N-35UH Neodymium Iron Boron Magnetic Material |