Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 18 - 20 MGOe | 18 - 20 MGOe | |
Ceradyne SEMICORE® S1-5A MMOA 20/15 SmCo5 Samarium Cobalt Magnet Magnetic alignment at 90° to Compaction AxisApplications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Herm.. |
|||
Magnetic Maximum Energy Product, BH | 16 - 20 MGOe | 16 - 20 MGOe | |
Ceradyne SEMICORE® S2-17C Specials Sm2 (CoFeCuZr)17 Samarium Cobalt Magnet Applications:Microwave amplifiers and oscillators for airborne equipmentTWT modules for phased array radarSmall motors for severe thermal conditions Hermetic magnetic couplings to replace shaft seal.. |