Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 40 - 43 MGOe | 40 - 43 MGOe | |
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 40 - 43 MGOe | 40 - 43 MGOe | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 40 - 43 MGOe | 40 - 43 MGOe | |
Alliance N-42SH Neodymium Iron Boron Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 40 - 43 MGOe | 40 - 43 MGOe | |
Alliance N-42H Neodymium Iron Boron Magnetic Material |