Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Maximum Energy Product, BH | 30 MGOe | 30 MGOe | |
Alliance S-30A Samarium Cobalt Magnetic Material |
|||
Magnetic Maximum Energy Product, BH | 30 MGOe | 30 MGOe | |
Alliance S-30B Samarium Cobalt Magnetic Material |