Electrical Properties | Metric | English | Comments |
---|---|---|---|
Tribocharge | 10 V | 10 V | Nitrile Glove |
Lubrizol Stat-Rite® S-102 Static Control Polypropylene Stat-Rite® S-102 is a static dissipative Polyethylene alloy. Stat-Rite® S-102 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Tribocharge | 10 V | 10 V | Nitrile Glove - BFG Test Method |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Tribocharge | 10 V | 10 V | Nitrile Glove - BFG Test Method |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Tribocharge | 10 V | 10 V | Nitrile Glove - BFG Test Method |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |