Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 8.51e+12 ohm @Time 86400 sec |
8.51e+12 ohm @Time 24.0 hour |
Telcordia GR-78, Control; IPC B25A |
Indium Corp. WF-9942 Wave Solder Flux, No-Residue WF-9942 Wave Soldering Flux is a no-clean flux specifically developed for wave soldering, mixed-technology and through-hole electronic assemblies. This formulations provides greater heat stability .. |