Electrical Properties | Metric | English | Comments |
---|---|---|---|
Track Resistance | 3600 - 36000 sec | 3600 - 36000 sec | Average value: 22300 sec Grade Count:17 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |