Electrical Properties | Metric | English | Comments |
---|---|---|---|
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB3000-20NY Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Track Resistance | 6000 sec | 6000 sec | Inclined-Plane Tracking; ASTM D2303 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |