Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000130 ohm-cm @Temperature 600 °C |
0.000130 ohm-cm @Temperature 1110 °F |
|
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750) Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 982 °C |
0.000130 ohm-cm @Temperature 1800 °F |
|
Carlson C 825 Nickel-Iron-Chromium Alloy General DescriptionCarlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion st.. |
|||
Electrical Resistivity | 0.000130 ohm-cm @Temperature 200 °C |
0.000130 ohm-cm @Temperature 392 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |