Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0001158 ohm-cm @Temperature 21.0 °C |
0.0001158 ohm-cm @Temperature 69.8 °F |
|
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |