Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000111 ohm-cm @Temperature 300 °C |
0.000111 ohm-cm @Temperature 572 °F |
Temperature resistance factor (F) =1.028 |
Alloy Wire International RW 80 Ni-Cr Resistance Wire Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations.. |
|||
Electrical Resistivity | 0.000111 ohm-cm @Temperature 700 °C |
0.000111 ohm-cm @Temperature 1290 °F |
|
ATI Allegheny Ludlum AL 403™ Martensitic Stainless Steel Characteristics: corrosion resistant, heat resistant, oxidation resistant up to 1400°F.Information provided by Allegheny Ludlum |
|||
Electrical Resistivity | 0.000111 ohm-cm @Temperature 20.0 °C |
0.000111 ohm-cm @Temperature 68.0 °F |
|
ATI Allegheny Ludlum ALFA-I™ Stainless Steel Type 406 Characteristics:superior oxidation resistance for the temperature range 1600°F-over 2200°F, high electrical resistivity, high resistance to sulfidation, high resistance to carburization. Applicat.. |