Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.000110 ohm-cm @Temperature 316 °C |
0.000110 ohm-cm @Temperature 601 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |
|||
Electrical Resistivity | 0.000110 ohm-cm @Temperature 200 °C |
0.000110 ohm-cm @Temperature 392 °F |
Temperature resistance factor (F) =1.015 |
Alloy Wire International RW 80 Ni-Cr Resistance Wire Used in heating elements and control resistors because of its electrical properties and resistance to oxidation under temperature cycling and frequent switching. Also used in hot cutting operations.. |