Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX DS0036I PC LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No.. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Faradex ZX93134 PPE+PS (Europe-Africa-Middle East) LNP* Faradex* ZX93134 is a compound based on PPE+PS Blend resin containing Stainless Steel Fiber and Glass Fiber. Added features include: Electrically Conductive, EMI/RFI Shielding.This data was su.. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP LUBRICOMP 9X06030 PA 46 (Europe-Africa-Middle East) LNP* LUBRICOMP* 9X06030 is a compound based on PA46 resin containing PTFE and Carbon Fiber. Added features include: Internally Lubricated, Heat Stabilized. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Europe-Africa-Middle East) LNP* Lubricomp* OCL4036L is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Surface Resistance | 1.0 - 1000 ohm | 1.0 - 1000 ohm | ASTM D257 |
Techmer ES Electrablend® PC 04006 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackInformation provided by TP Composite.. |
|||
Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D257 |
Techmer ES Electrafil® J-1/CF/30/TF/13/SI/2 Nylon 66, 30% Carbon Fiber, 13% PTFE, 2% Silicone |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DE0049F PC LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding... |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA.. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC (Europe-Africa-Middle East) LNP* STATKON* DEL36 is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated. |
|||
Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East) LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON UEF26AS PPA (Europe-Africa-Middle East) LNP* Stat-kon* UEF26AS is a compound based on Polyphthalamide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP EC008 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EC008 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | IEC 60093 |
Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica.. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East) LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WC006 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
Surface Resistance | 100 - 1000 ohm | 100 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05042 PC (Europe-Africa-Middle East) LNP* Stat-kon* DX05042 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific) LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East) LNP* Stat-kon* DE006P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the .. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East) LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified. |
|||
Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |