Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 9.00e+16 ohm | 9.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 3105H Polybutylene Terephthalate (PBT), Standard, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 9.00e+16 ohm | 9.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 751SA Polybutylene Terephthalate (PBT), Low density, Low wear, GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |