Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 5.01e+9 ohm | 5.01e+9 ohm | ASTM D257 |
Tipco Tipcolite® TG 618 Phenolic Compound, Mineral & Wood Flour, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: Electrical & ElectronicsProcessing: Compression & TransferInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Surface Resistance | 5.01e+9 ohm | 5.01e+9 ohm | ASTM D257 |
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Switchgear, HRC FusesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |