Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 4.50e+13 ohm | 4.50e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD250C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.50) with Tight Tolerance.. |
|||
Surface Resistance | 4.50e+13 ohm | 4.50e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD255C PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Very Low Loss PTFE and Ceramic Filled Composite (0.0014 Loss Tangent at 10GHz and Base Station Frequencies)Dielectric Constant (2.55) with Tighter Toleran.. |
|||
Surface Resistance | 4.50e+13 ohm | 4.50e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD260A PTFE/Woven Fiberglass/Microdispersed Ceramic Filled Laminate for RF & Microwave PCBs For RF & Microwave Printed Circuit Boards. Low Loss PTFE and Ceramic Filled Composite Dielectric Constant (2.60)Low Dielectric Loss (Loss Tangent)Low Profile Copper (lower conductive losses)Low Z-d.. |
|||
Surface Resistance | 4.50e+13 ohm | 4.50e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon AD350A PTFE/Woven Fiberglass/Ceramic Filled Composite Tighter Dielectric Tolerance Low Z-Axis Thermal ExpansionCeramic Filled PTFEHigh Thermal ConductivityLarge Panel SizeBenefits:Higher Consistency of PerformanceSuperior PTH AdhesionHeat Dissipation a.. |
|||
Surface Resistance | 4.50e+13 ohm | 4.50e+13 ohm | C96/35/90; IPC TM-650 2.5.17.1 |
Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates DiClad 522 and DiClad 527 use a higher fiberglass/PTFE ratio to provide mechanical properties approaching conventional substrates.Extremely Low Loss TangentExcellent Dimensional StabilityProduct Per.. |