Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.10e+15 ohm | 3.10e+15 ohm | ASTM D257 |
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Surface Resistance | 3.10e+15 ohm | 3.10e+15 ohm | ASTM D257 |
Arkema Group Orgalloy® LT 5050 Polyamide Alloy Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Surface Resistance | 3.10e+15 ohm | 3.10e+15 ohm | ASTM D257 |
Arkema Group Orgalloy® RS 6010 Polyamide 6 Alloy 10% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Surface Resistance | 3.10e+15 ohm | 3.10e+15 ohm | ASTM D257 |
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group |