Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+8 ohm | 2.00e+8 ohm | TM650 2.5.17.1 |
Premix Thermoplastics PREBOARD E1025 Standard Epoxy Circuit Boards Standard epoxy (FR4) circuit boards do not lend themselves for high frequency applications due to the poor dielectric properties. For that reason PTFE is used predominately. This is an expensive mat.. |
|||
Surface Resistance | 2.00e+8 ohm | 2.00e+8 ohm | TM650 2.5.17.1 |
Premix Thermoplastics PREBOARD E1026 Standard Epoxy Circuit Boards PREBOARD is a thermoplastic based PCB laminate. Low dissipation factor leads to high gain in the antennas. As a non filled laminate PREBOARD is fully homogenous so that consistant properties are ac.. |
|||
Surface Resistance | 2.00e+8 ohm @Temperature 90.0 °C |
2.00e+8 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Surface Resistance | 2.00e+8 ohm | 2.00e+8 ohm | |
LATI Latistat 62-08 PA6 Dissipative product based on Polyamide 6 (PA6). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.. |
|||
Surface Resistance | 2.00e+8 ohm | 2.00e+8 ohm | ASTM D257 |
Tipco Tipcolite® TG 613 Phenolic Compound, Mineral & Wood Flour, Soft Flow & Good Surface Finish Soft Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: General PurposeProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Surface Resistance | 2.00e+8 ohm | 2.00e+8 ohm | DIN 53482 |
DSM Fibre Intermediates Nyrim® 4000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Surface Resistance | 2.00e+8 ohm @Temperature 90.0 °C |
2.00e+8 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Chevron Phillips Ryton® R10 7006A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |