Electrical Properties Metric English Comments
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
ASTM D257
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded  
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d..
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
IEC 60093
Polyplastics Duracon® TR-5 Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
IEC 60093
Polyplastics Duranex® 7400W Polybutylene Terephthalate (PBT), Super low warpage, GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
ASTM D257
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part ..
Surface Resistance 2.00e+15 ohm
2.00e+15 ohm
ASTM D257
Solvay Specialty Polymers Amodel® AF-1145 V0 Polyphthalamide (PPA) Resin, 45% Glass Reinforced, Dry As Molded  
AMODEL AF-1145 V0 is a 45% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high heat distortion temperature, high tensile strength and flexural modulus. The material is rela..