Electrical Properties Metric English Comments
Surface Resistance 1.90e+16 ohm
1.90e+16 ohm
ASTM D 257
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East)
XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid..