Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1e+05 - 1.00e+7 ohm | 1e+05 - 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | Teil 30; IEC 60093 / VDE 0303 |
Okulen® 1000 PE-UHMW, AST OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | 400 um thick sheet; ISO D-257 |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+8 ohm | 1.00e+7 - 1.00e+8 ohm | 1 volt; ASTM D4496 |
Omni Plastics OmniTech™ CPP XE65 BK12 ESD Polypropylene Dissipative OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Surface Resistance | 1.00e+7 - 1.00e+17 ohm | 1.00e+7 - 1.00e+17 ohm | Average value: 2.12e+16 ohm Grade Count:26 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+14 ohm | 1.00e+7 - 1.00e+14 ohm | Average value: 1.49e+13 ohm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105-8422 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1850-7854 PBT, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | |
LATI Latiohm 83-07 PD11 CNT PA12, Impact Modified Semiconductive/dissipative product based on Polyamide 12 (PA12), impact modified. Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 LNP* STAT-KON* REP349 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone, 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON REP349 PA 66 (Asia Pacific) LNP* Stat-kon* REP349 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Surface Resistance | 1.00e+7 - 1.00e+9 ohm | 1.00e+7 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS LNP* STAT-LOY* AX11421 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Surface Resistance | 1.00e+7 - 1.00e+11 ohm | 1.00e+7 - 1.00e+11 ohm | Dry; ASTM D257 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | 40% let-down in HDPE |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | 40% let-down in HDPE |
A. Schulman POLYBLAK™ 4663 Premium Conductive 40% Carbon Black Concentrate Based In Modified HDPE DescriptionPOLYBLAK® Black 4663 is a premium conductive carbon black concentrate containing 40% carbon black based in a modified HDPE carrier resin. This masterbatch is designed to provide a flexi.. |
|||
Surface Resistance | <= 1.00e+7 ohm @Temperature 23.0 °C |
<= 1.00e+7 ohm @Temperature 73.4 °F |
IEC 60093 |
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | DIN IEC 60093 |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | DIN IEC 60093 |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Surface Resistance | 1.00e+7 ohm | 1.00e+7 ohm | ASTM D257 |
Techmer ES Statiblend® PPS GF35 SS7 BK 35/7% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel Fiber, 35/7% Filler by WeightUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | <= 1.00e+7 ohm | <= 1.00e+7 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PA 1406 PRE-ELEC PA 1406 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon fiber. In addition to a low electrical resistivity PRE-ELEC PA 1406 .. |