Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | IEC 60093 |
PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | 400 um thick sheet; ISO D-257 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 93 |
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Surface Resistance | 1.00e+6 - 5.00e+16 ohm | 1.00e+6 - 5.00e+16 ohm | Average value: 6.27e+15 ohm Grade Count:23 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1105-8004 PEEK, with carbon fiber, low-warpage, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically .. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | ASTM D257 |
LG Chemical LUCON PO-5300M Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | ASTM D257 |
LG Chemical LUCON SE-4200H Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | ASTM D4496 |
Techmer ES Electrafil® J-50/CF/10 Polycarbonate, 10% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DFD029 PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD029 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Reta.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX04403 PC LNP STAT-KON* DX04403 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Surface Resistance | 1.00e+6 - 1.00e+8 ohm | 1.00e+6 - 1.00e+8 ohm | ASTM D257 |
Techmer ES Statiblend® PA12 CB Availability: North AmericaForms: PelletsAdditive: Carbon BlackFeatures: ConductiveAppearance: BlackTPCI# 9872105Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
EMS-Grivory Grivory® L 25 NZ ESD PA12 Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of .. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
EMS-Grivory Grivory® LV-3 ESD PA12-GF30 Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where.. |