Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+8 - 8.00e+15 ohm | 1.00e+8 - 8.00e+15 ohm | Average value: 8.06e+14 ohm Grade Count:38 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |