Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+13 - 7.30e+17 ohm | 1.00e+13 - 7.30e+17 ohm | Average value: 8.24e+16 ohm Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |