Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+12 - 5.00e+13 ohm @Temperature 90.0 - 90.0 °C |
1.00e+12 - 5.00e+13 ohm @Temperature 194 - 194 °F |
Average value: 1.73e+13 ohm Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Surface Resistance | 3.00e+13 - 5.00e+13 ohm | 3.00e+13 - 5.00e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Surface Resistance | 3.00e+13 - 5.00e+13 ohm | 3.00e+13 - 5.00e+13 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |