Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 - 1.00e+17 ohm | 1.00e+14 - 1.00e+17 ohm | Average value: 8.01e+15 ohm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+17 ohm | 1.00e+8 - 1.00e+17 ohm | Average value: 3.60e+15 ohm Grade Count:34 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Surface Resistance | 1000 - 1.00e+17 ohm | 1000 - 1.00e+17 ohm | Average value: 5.23e+15 ohm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+17 ohm | 1.00e+6 - 1.00e+17 ohm | Average value: 7.79e+15 ohm Grade Count:36 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Surface Resistance | 1.00e+15 - 1.00e+17 ohm | 1.00e+15 - 1.00e+17 ohm | Average value: 3.70e+16 ohm Grade Count:3 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+17 ohm | 1.00e+14 - 1.00e+17 ohm | Average value: 4.74e+16 ohm Grade Count:17 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+17 ohm | 1.00e+14 - 1.00e+17 ohm | Average value: 1.50e+16 ohm Grade Count:34 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Surface Resistance | 100 - 1.00e+17 ohm | 100 - 1.00e+17 ohm | Average value: 5.52e+15 ohm Grade Count:23 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+17 ohm | 1.00e+15 - 1.00e+17 ohm | Average value: 1.75e+16 ohm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Surface Resistance | 10.0 - 1.00e+17 ohm | 10.0 - 1.00e+17 ohm | Average value: 6.89e+15 ohm Grade Count:37 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Surface Resistance | 1.00e+7 - 1.00e+17 ohm | 1.00e+7 - 1.00e+17 ohm | Average value: 2.12e+16 ohm Grade Count:26 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+17 ohm | 1.00e+11 - 1.00e+17 ohm | Average value: 9.84e+15 ohm Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Surface Resistance | 1.00e+15 - 1.00e+17 ohm | 1.00e+15 - 1.00e+17 ohm | Average value: 1.73e+16 ohm Grade Count:14 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00e+12 - 1.00e+17 ohm | 1.00e+12 - 1.00e+17 ohm | Average value: 5.25e+16 ohm Grade Count:4 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Surface Resistance | 10000 - 1.00e+17 ohm | 10000 - 1.00e+17 ohm | Average value: 2.50e+16 ohm Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim.. |
|||
Surface Resistance | 0.200 - 1.00e+17 ohm | 0.200 - 1.00e+17 ohm | Average value: 2.24e+15 ohm Grade Count:45 |
Overview of materials for Polyether Block Amide (PEBA) This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+17 ohm | 1.00e+13 - 1.00e+17 ohm | Average value: 2.92e+16 ohm Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+17 ohm | 1.00e+13 - 1.00e+17 ohm | Average value: 5.27e+16 ohm Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Surface Resistance | 10000 - 1.00e+17 ohm | 10000 - 1.00e+17 ohm | Average value: 4.62e+15 ohm Grade Count:27 |
Overview of materials for Polyimide, Thermoset Film This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+17 ohm | 1.00e+13 - 1.00e+17 ohm | Average value: 1.34e+16 ohm Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |