Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IEC 60093 |
Raschig Group RALUPOL® 5000 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all.. |
|||
Surface Resistance | 1.50e+10 - 1.00e+12 ohm | 1.50e+10 - 1.00e+12 ohm | Average value: 3.04e+11 ohm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Surface Resistance | 5.00e+8 - 1.00e+12 ohm | 5.00e+8 - 1.00e+12 ohm | Average value: 2.78e+11 ohm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Surface Resistance | 1.00 - 1.00e+12 ohm | 1.00 - 1.00e+12 ohm | Average value: 1.44e+10 ohm Grade Count:92 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Surface Resistance | 0.100 - 1.00e+12 ohm | 0.100 - 1.00e+12 ohm | Average value: 1.30e+10 ohm Grade Count:69 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Surface Resistance | 10000 - 1.00e+12 ohm | 10000 - 1.00e+12 ohm | Average value: 3.50e+11 ohm Grade Count:3 |
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Surface Resistance | 1000 - 1.00e+12 ohm | 1000 - 1.00e+12 ohm | Average value: 3.33e+11 ohm Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East) LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 9X03508 PPO+PA66 LNP* STAT-LOY* 9X03508 is a compound based on PPO+PA66 resin containing Proprietary Filler(s). Added features of this material include: Antistatic, Flame Retardant, High Impact. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS (Europe-Africa-Middle East) LNP* Stat-loy* A3000 is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX05015 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX05015 is a compound based on Acetal Copolymer resin containing Antistat. Added features include permanent Anti-Static. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® 02056 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9111116Information provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY NX03583 PC+ABS LNP STAT-LOY* NX03583 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Surface Resistance | 4000 - 1.00e+12 ohm | 4000 - 1.00e+12 ohm | Average value: 1.17e+11 ohm Grade Count:9 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D 257 |
SABIC Innovative Plastics Valox® VC108 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Surface Resistance | 1.00e+10 - 1.00e+12 ohm | 1.00e+10 - 1.00e+12 ohm | Average value: 1.04e+11 ohm Grade Count:11 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | ASTM D257 |
Supreme Petrochem SP 6630 Antistatic Polystyrene Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti.. |
|||
Surface Resistance | 1.00e+8 - 1.00e+12 ohm | 1.00e+8 - 1.00e+12 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific) Polycarbonate base, 8% carbon fiber reinforced, FR |