Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 7.30e+17 ohm | 7.30e+17 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |