Polymer Property : Surface Resistance = 7.00e+11 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 7.00e+11 ohm
7.00e+11 ohm
XXX Phenolic Laminate
Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b..