Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-30-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | ASTM D249 |
PlastxWorld CEVIAN® EG506 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | |
Covestro Desmopan® 588 Thermoplastic Polyurethane Desmopan 588 is a TPU on the basis of a special ether with good microbe-resistance.Applications: Cable sheathing, hoses, profiles.Information provided by Bayer.As of 1 September 2015, Bayer Material.. |
|||
Surface Resistance | 6.00e+11 ohm | 6.00e+11 ohm | |
Covestro Desmopan® 786 Thermoplastic Polyurethane Desmopan 786 is a TPU on the basis of a special carbonate with very good microbe-resistance.Applications: Tabular films, films, profiles.Information provided by Bayer.As of 1 September 2015, Bayer M.. |