Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 48 ohm | 48 ohm | |
LATI Latishield 73/13-07A POM, Steel Fiber Reinforced EMI shielding product based on Polyoxymethylene (POM). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |