Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.00e+15 - 3.00e+16 ohm | 3.00e+15 - 3.00e+16 ohm | IEC 60093 |
Polycasa AKRYLON XT PMMA AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT .. |
|||
Surface Resistance | 3.00e+15 - 3.00e+16 ohm | 3.00e+15 - 3.00e+16 ohm | IEC 60093 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Surface Resistance | 3.00e+15 ohm | 3.00e+15 ohm | IEC 60093 |
Polyplastics Duracon® TD-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 3.00e+15 ohm | 3.00e+15 ohm | IEC 60093 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |