Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.86e+17 ohm | 2.86e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Surface Resistance | 2.86e+17 ohm | 2.86e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Surface Resistance | 2.86e+17 ohm | 2.86e+17 ohm | ASTM D 257 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |