Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade Amber pelletsInformation provided by Infinite Polymer System II. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | 500V; Ø 93x3mm; IEC 60093 |
SYNTHOS Forsan® 548 Acrylonitrile Butadiene Styrene (ABS) Easy flow, glossy, impact resistant.Applications: General purposeVarious technical parts, household appliances, hobby and office equipment, etc.Synthos was formerly known as Kaucuk. All information .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 303RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 313RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duracon® TR-10D Acetal Co-polymer (POM), Mineral filling, Mineral filling, High rigidity, Low warpage DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 3306 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duranex® 3400 Polybutylene Terephthalate (PBT), Standard, 40% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | |
Loctite® 3534 Glob Top Encapsulant COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | ASTM D257 |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | Average value: 2.00e+16 ohm Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |
|||
Surface Resistance | 2.00e+16 ohm | 2.00e+16 ohm | IEC 60093 |
Polyplastics Duracon® GH-25 Acetal Co-polymer (POM), GF 25% reinforced, High strength, High rigidity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |