Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Test 2 |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | ROA; IEC 60093 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | |
Covestro Baydur® 40 Polyurethane Rigid integral skin polyurethane foam for lightweight moldings. Sandwich structure gives a high stiffness-to-weight ratio.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience .. |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1010N2 1ES NAT PA6 FR(30) Injection Molding, Flame Retardant (Halogen free) |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1013C5 PA6 Injection Molding, Easy Molding Grade |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1013G30 1 NA PA6-GF30 30% Glass Reinforced, Injection Molding |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | cond; IEC 60093 |
DSM Novamid® 1015G33-8 NAT PA6-GF33 33% Glass Reinforced, Injection Molding |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | IEC 60093 |
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | |
Reliance Industries PVAXX H60 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |
|||
Surface Resistance | 2.00e+14 ohm | 2.00e+14 ohm | Test 2 |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |