Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.90e+16 ohm | 1.90e+16 ohm | ASTM D 257 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |