Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.69e+13 ohm | 1.69e+13 ohm | |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |