Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1.00e+6 ohm @Thickness 0.400 mm |
<= 1.00e+6 ohm @Thickness 0.0157 in |
ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® PS 1331 Carbon Black Filled Conductive Thermoplastic Compound PRE-ELEC® PS 1331 is a carbon black filled conductive thermoplastic compound based on polystyrene. In addition to a low electrical resistivity PRE-ELEC® PS 1331 has excellent mechanical properties.. |
|||
Surface Resistance | <= 1.00e+6 ohm @Thickness 3.00 mm |
<= 1.00e+6 ohm @Thickness 0.118 in |
ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® TPE 1501 Conductive Thermoplastic Compound PRE-ELEC® TPE 1501 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+7 ohm @Thickness 2.00 mm |
1.00e+6 - 1.00e+7 ohm @Thickness 0.0787 in |
sheet; IEC 61340-5-1 |
Panipol Oy DXH-PP Inherently Conductive Polymer Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr.. |
|||
Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | |
Nilit FRIANYL A63 CV15 Nylon 6.6 for injection molding, 15% carbon fiber reinforced Nylon 6.6 for injection molding (good electrical conductivity and antistatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | ASTM D257 |
PolyOne Edgetek® RA-10GF-10CF/000 HI Polyphenylsulfone (PPSU) Information provided by PolyOne |
|||
Surface Resistance | 1.00e+6 - 1.00e+15 ohm | 1.00e+6 - 1.00e+15 ohm | Average value: 4.54e+14 ohm Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | ISO D-257 |
Premix Thermoplastics PRE-ELEC® PPE 1462
(discontinued **) PRE-ELEC PPE 1462 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 93 |
LATI LATISTAT 30/R-05 High Impact Strength Polystyrene Base Conductive Plastic
(discontinued **) Description: Latistat materials have low specific resistivity. They feature partial electrical conductivity. Selected functional additives give materials with low specific resistivity and reasonable.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+8 ohm | 1.00e+6 - 1.00e+8 ohm | ASTM D257 |
LNP ULTEM® JD7902 Polyetherimide
(discontinued **) Forms: PelletsInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1105-8279 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Surface Resistance | <= 1.00e+6 ohm | <= 1.00e+6 ohm | |
Lehmann & Voss LUVOCOM® 80-7626 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DFD029 PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD029 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Reta.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+10 ohm | 1.00e+6 - 1.00e+10 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1508 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_HMC1508 compound is a static dissipative NORYL resin. |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY AF306 ABS LNP* STAT-LOY* AF306 is a compound based on ABS resin containing 30% Glass Fiber. Added feature of this material is: Antistatic. |
|||
Surface Resistance | 1.00e+6 - 1.00e+9 ohm | 1.00e+6 - 1.00e+9 ohm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX04462C PC (Asia Pacific) LNP* STAT-KON* DX04462C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20 Information provided by EMS Grivory |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | ASTM D257 |
Adamas Adalon® 503 PTFE, 0.1% MoS2 Information provided by Adamas, HPM |
|||
Surface Resistance | 1.00e+6 ohm | 1.00e+6 ohm | IEC 60093 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Surface Resistance | 1e+05 - 1.00e+6 ohm | 1e+05 - 1.00e+6 ohm | IEC 60093 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |