Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | <= 1.00e+11 ohm @Thickness 3.00 mm |
<= 1.00e+11 ohm @Thickness 0.118 in |
molded plate; ISO IEC 61340-5-1 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53 482 |
Perstorp Compounds Aminel GF Melamine Fiberglass-reinforced melamine material with high dimensional stability, excellent injection properties and high thermal stabilityInformation provided by Perstorp Compounds Inc. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Surface Resistance | 1.00e+11 ohm @Temperature 90.0 °C |
1.00e+11 ohm @Temperature 194 °F |
95% RH, 48 hrs |
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev.. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | |
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Lanxess Durethan® C 38 FKS 000000 Copolyamide Copolyamide, film quality, high transparency, with processing aid, nucleatedApplication Examples: blown film coextrusion (outer layer) |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 218 V20 Black 21N PA66, 20% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 20% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 218 V20 is used in all sectors of industry.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 222 Black 1N PA66, Conditioned Description: Unreinforced polyamide PA66, medium viscosity, heat stabilized, for injection molding, fast crystallization, for short cycles .Available in: EuropeProduct Applications: TECHNYL A 222 of.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 402 Natural FA PA66, Conditioned Description: Unreinforced polyamide PA66, very high viscosity, for extrusion.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 402 NATURAL FA offers three main advantages: hi.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® C 216 V40 PA6, 40% glass fiber, Conditioned Description: TECHNYL® C 216 V40 is a polyamide 6, reinforced with 40% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers a good combinati.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | ASTM D257 |
Techmer ES HiFill® PA6/6 GF33 BK024 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, Conditioned Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
DSM Arnitel® EM740 Polyether Ester Elastomer (European Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® BS PA6 Product description: Grilon BS is an unreinforced, heat stabilized standard PA6 injection molding grade with normal melt viscosity. Grilon BS has the following important properties: Good flow behavi.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® XE 4108 nat PA612-GF50 Product description: Grilamid XE 4108 natural is a 50% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4108 are: low water absorptiong.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30 Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
EMS-Grivory Grivory® LBV-65H FWA nat PA12-GF65 Product description: Grilamid LBV-65H FWA natural is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | CEI 60093 |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Barlog Plastics KEBATER A0230 PBT/ABS, 30% glass fiber reinforced, low warpage (PBT+ABS)-GF30Information provided by BARLOG plastics GmbH. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | DIN 53482/VDE 0303 |
BASF Elastollan® C-95A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+12 ohm | 1.00e+11 - 1.00e+12 ohm | IS 3396-1979 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Surface Resistance | >= 1.00e+11 ohm | >= 1.00e+11 ohm | IS 3396-1979 |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Surface Resistance | 1.00e+11 - 3.16e+11 ohm | 1.00e+11 - 3.16e+11 ohm | IS 3396-1979 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
Bulk Molding Compounds tetra-DUR F 4001 Bulk Molding Compound UL-Licensed, Abrasion resistance, free of fiber glass.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipati.. |
|||
Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | Conditioned; CEI 60093 |
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast. |