Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 4000 V @Thickness 1.57 mm |
4000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP320E Cotton Fabric Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500†|
|||
Dielectric Breakdown | 4000 V @Thickness 1.57 mm |
4000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP318 Cotton Fabric Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t.. |