Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 35000 V @Thickness 1.57 mm |
35000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP159 Synthetic Fabric
(discontinued **) Description: Woven aramid fiber fabric combined with high temperature phenolic resin. With a proper post baking procedure, NP159 will withstand continuous operation at 200° C. Material becomes brit.. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 35000 V @Temperature 194 °F, Time 0.00556 hour |
Step -by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe SI GC 21 Woven Glass Cloth Reinforced Silicone Resin - Round, Rolled Tube Good mechanical, electrical and electronic applications when exposed to high relative humidity.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 35000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 35000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe SI GC 21 Woven Glass Cloth Reinforced Silicone Resin - Round, Rolled Tube Good mechanical, electrical and electronic applications when exposed to high relative humidity.Information provided by Hippe. |