Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | 15000 V @Thickness 0.125 mm |
15000 V @Thickness 0.00492 in |
1/4 inch electrode; ASTM D149 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Dielectric Breakdown | 15000 V @Thickness 0.100 mm |
15000 V @Thickness 0.00394 in |
ASTM D149 |
Victrex® APTIV® 2000-050 Polyetheretherketone (PEEK) Polymer Film, Amorphous APTIV PEEK 2000 series films are the unfilled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTIV PEEK .. |
|||
Dielectric Breakdown | >= 15000 V @Temperature 90.0 - 90.0 °C |
>= 15000 V @Temperature 194 - 194 °F |
Average value: 15000 V Grade Count:1 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Breakdown | >= 15000 V @Time 20.0 - 60.0 sec |
>= 15000 V @Time 0.00556 - 0.0167 hour |
Average value: 15000 V Grade Count:1 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Dielectric Breakdown | 15000 V @Thickness 0.250 mm |
15000 V @Thickness 0.00984 in |
ASTM D149 |
Mapal Plastics Maplon CFA-HK Polypropylene Sheet Applications: For use with electrical insulation products. For use when flame retardant and static dissipative properties are required. |
|||
Dielectric Breakdown | 15000 V @Thickness 1.57 mm |
15000 V @Thickness 0.0620 in |
Cond D-48/50; ASTM D229 S/S |
Industrial Laminates/Norplex NP504 Glass Fabric Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note.. |
|||
Dielectric Breakdown | 15000 V @Thickness 1.57 mm |
15000 V @Thickness 0.0620 in |
D-48/50 |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Dielectric Breakdown | 15000 V @Thickness 1.00 mm |
15000 V @Thickness 0.0394 in |
|
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Dielectric Breakdown | >= 15000 V @Temperature 90.0 °C, Time 20.0 sec |
>= 15000 V @Temperature 194 °F, Time 0.00556 hour |
Step-by-step test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 15000 V @Temperature 90.0 °C, Time 60.0 sec |
>= 15000 V @Temperature 194 °F, Time 0.0167 hour |
Proof test, In oil, parallel to laminations; IEC 1212-2 5.1 |
Hippe PF GC 21 Woven Glass Cloth Reinforced Phenolic Resin - Round, Rolled Tube Used in mechanical, electrical and electronic applications. Very high mechanical strength at moderate temperatures.Information provided by Hippe. |
|||
Dielectric Breakdown | 15000 V @Thickness 1.00 mm |
15000 V @Thickness 0.0394 in |
ASTM-D149 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |