Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+12 - 5.60e+16 ohm-cm | 1.00e+12 - 5.60e+16 ohm-cm | Average value: 9.96e+15 ohm-cm Grade Count:45 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |