Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+13 - 3.30e+17 ohm-cm | 1.00e+13 - 3.30e+17 ohm-cm | Average value: 2.04e+16 ohm-cm Grade Count:34 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |