Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 100 - 1.30e+13 ohm-cm | 100 - 1.30e+13 ohm-cm | Average value: 1.00e+12 ohm-cm Grade Count:5 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |