Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00 - 1.00e+9 ohm-cm | 1.00 - 1.00e+9 ohm-cm | Average value: 8.33e+7 ohm-cm Grade Count:17 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Electrical Resistivity | 5.00 - 1.00e+9 ohm-cm | 5.00 - 1.00e+9 ohm-cm | Average value: 7.19e+7 ohm-cm Grade Count:15 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Electrical Resistivity | 10.0 - 1.00e+9 ohm-cm | 10.0 - 1.00e+9 ohm-cm | Average value: 5.67e+7 ohm-cm Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |