Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | IEC 60093 |
Murtfeldt Murflor® Polytetrafluoroethylene, 25% Carbon The integration of 25% carbon increases the wear resistance, hardness, and creep strength of this material. Murflor® + Carbon is used, for example, when electrical conductivity is required and Mate.. |
|||
Electrical Resistivity | 1.00 - 1.00e+6 ohm-cm | 1.00 - 1.00e+6 ohm-cm | Average value: 270000 ohm-cm Grade Count:35 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Electrical Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Average value: 500000 ohm-cm Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m.. |
|||
Electrical Resistivity | 10000 - 1.00e+6 ohm-cm | 10000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Average value: 117000 ohm-cm Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Electrical Resistivity | 1.00 - 1.00e+6 ohm-cm | 1.00 - 1.00e+6 ohm-cm | Average value: 143000 ohm-cm Grade Count:10 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Electrical Resistivity | 100 - 1.00e+6 ohm-cm @Temperature 20.0 °C |
100 - 1.00e+6 ohm-cm @Temperature 68.0 °F |
|
Acerde Silicon Carbide Silicon Carbide key properties: High oxidation resistance, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, High elastic modulus, Superior chemical inert.. |
|||
Electrical Resistivity | 0.0500 - 1.00e+6 ohm-cm | 0.0500 - 1.00e+6 ohm-cm | doped |
Mateck Zinc Selenide, ZnSe Semiconductor single crystals. Twins and stacking faults twin free. |