Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.00e+10 - 1.00e+13 ohm-cm | 1.00e+10 - 1.00e+13 ohm-cm | Average value: 3.37e+12 ohm-cm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+13 ohm-cm | 1.00e+11 - 1.00e+13 ohm-cm | Average value: 4.26e+12 ohm-cm Grade Count:15 |
Overview of materials for Phenolic; Unreinforced; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Electrical Resistivity | 1.00 - 1.00e+13 ohm-cm | 1.00 - 1.00e+13 ohm-cm | Average value: 4.17e+11 ohm-cm Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Electrical Resistivity | 1.00e+11 - 1.00e+13 ohm-cm | 1.00e+11 - 1.00e+13 ohm-cm | Average value: 3.70e+12 ohm-cm Grade Count:3 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |